Sarkar, Ritwik and Banerjee, Goutam (1999) Densification study of attritor milled magnesium aluminate spinel. Transactions of the Indian Ceramic Society, 58 (4). 92-94,103. ISSN 0371-750X

[img] PDF - Published Version
Restricted to Registered users only

Download (354Kb) | Request a copy

Abstract

Pre-synthesization of magnesium aluminate spinel was done by mixing magnesium hydroxide and aluminium hydroxide in a molar ratio of MgO: Al2O3 = 1:1 and then calcining the mixture at temperatures between 900° and 1600°C. X-ray diffraction patterns confirmed that only spinel phase was present above 1400°C. Pre-synthesized spinels were then attritor milled up to 6 h and the extent of milling was characterized by surface area measurement. Milled and unmilled materials were isostatically pressed at 175 MPa and sintered between 1550° and 1650°C for 2 h and studied for densification. A maximum of 99% densification was achieved at a sintering temperature of 1650°C.

Item Type: Article
Subjects: Refractories
Divisions: Refractory
Depositing User: Bidhan Chaudhuri
Date Deposited: 21 Jun 2012 10:39
Last Modified: 11 Mar 2014 12:24
URI: http://cgcri.csircentral.net/id/eprint/1543

Actions (login required)

View Item View Item