Karak, S K and Vishnu, C S and Witczak, Z and Lojkowsk, W and Dutta Majumdar, Jyotsna and Manna, Indranil (2010) Studies on wear behavior of nano-Y2O3 dispersed ferritic steel developed by mechanical alloying and hot isostatic pressing. Wear, 270 (1-2). pp. 5-11. ISSN 0043-1648
PDF
- Published Version
Restricted to Registered users only Download (1070Kb) | Request a copy |
Abstract
Resistance to wear is an important factor in design and selection of structural components in motion and in contact with a mating surface. The present work deals with studies on fretting wear behavior of mechanically alloyed 1.0 wt.% nano-Y2O3 dispersed 71.0Fe–25.5Cr–2.0Al–0.5Ti (wt.%) ferritic steel consolidated by hot isostatic pressing at 600, 800 and 1000 ◦C under 1.2 GPa uniaxial pressure applied for 1 h. The wear experiments were carried out in gross slip fretting regime against 6mmdiameter tungsten carbide ball at ambient temperature. The highest resistance to fretting wear has been observed in the alloy sintered at 1000 ◦C. The fretting involves localized plastic deformation and oxidation as evidenced by post wear surface profile and micro-compositional analysis, respectively.
Item Type: | Article |
---|---|
Uncontrolled Keywords: | Metal matrix composite;Hardness;Electron microscopy;Wear testing |
Subjects: | Engineering Materials |
Divisions: | UNSPECIFIED |
Depositing User: | Bidhan Chaudhuri |
Date Deposited: | 21 May 2012 07:43 |
Last Modified: | 21 May 2012 07:43 |
URI: | http://cgcri.csircentral.net/id/eprint/1421 |
Actions (login required)
View Item |