Sarkar, Ritwik and Bannerjee, Goutam (2000) Effect of addition of TiO2 on reaction sintered MgO-Al2O3 spinels. Journal of the European Ceramic Society, 20 (12). 2133-2141 . ISSN 0955-2219
PDF
- Published Version
Restricted to Registered users only Download (822Kb) | Request a copy |
Abstract
Three different spinel compositions with MgO:Al2O3 molar ratios 2:1, 1:1 and 1:2 were studied using TiO2 as an additive up to 2 wt.%. Solid state reaction sintering technique was employed for all the compositions in the temperature range of 1550-1650 degrees C. Attrition milling was done for the reduction of particle size. Sintered products were characterised in terms of densification and shrinkage studies, phase analysis, strength evaluation both at ambient temperature and at elevated temperature, strength retention after different number of thermal cycles at 1000 degrees C, quantitative elemental analysis and microstructural studies
Item Type: | Article |
---|---|
Uncontrolled Keywords: | MgA1(2)O(4); microstructure-final; sintering; spinels; TiO2 |
Subjects: | Microstructure and Characterization |
Divisions: | Refractory |
Depositing User: | Mrs Chandana Patra |
Date Deposited: | 06 Feb 2012 12:18 |
Last Modified: | 16 Mar 2012 06:30 |
URI: | http://cgcri.csircentral.net/id/eprint/662 |
Actions (login required)
View Item |