Sarkar, Ritwik and Mukherjee, S and Ghosh, A (2008) Effect of AlF3 on spinel formation. Industrial Ceramics , 28 (1). pp. 33-36. ISSN 1121-7588

Full text not available from this repository. (Request a copy)

Abstract

Spinel formation was studied by phase analysis and dilatomeric experiment using commercially available caustic magnesia and technical alumina in the temperature range of 1000 degrees C to 1400 degrees C. AlF3 as mineralizer was added up to 3 wt%. AlF3 was found to reduce the spinel formation temperature significantly, but also reduces the reactivity of the calcined products, measured by specific surface area.